Skip to main content
. 2019 Nov 20;10:5266. doi: 10.1038/s41467-019-13178-2

Fig. 3.

Fig. 3

Conductive behavior of Na2.88Sb0.88W0.12S4 electrolyte. a Conductivity at 25 °C (σ25) and activation energy Ea for the conduction of the pelletized Na2.88Sb0.88W0.12S4 electrolytes as a function of heat treatment (H.T.) time at 275 °C. The pellets were prepared by cold-pressing the electrolyte powder at 1080 MPa, followed by heat treatment at 275 °C. b The Arrhenius plot of the Na ion conductivity of the Na2.88Sb0.88W0.12S4 electrolyte developed in this study and representative Na ion conductors reported so far