(A) TEM image of PtPdMo nanocubes with an average size of 12.08 nm. (B) HRTEM image of PtPdMo nanocubes. The interplanar spacing of 0.225 nm is corresponding to (111) crystal plane, and the dislocation exists along the bounded ridge of nanocrystal labeled by red lines. (C) Hydrodynamic test of PtPdMo dissolved in 10% FBS at the concentration of 1 mg/mL. XPS spectra of (D) Pt 4f, (E) Pd 3d, and (F) Mo 3d in the PtPdMo nanocubes, respectively.