Skip to main content
. 2019 Nov 23;10(1):1. doi: 10.1007/s13205-019-1978-z

Table 2.

Glucose yield from glucan remaining in lignin isolates during hydrolysis

Type of LI (FPU g−1 LI) Glucose yield (g g−1)
CTec2 loading 0.25% LI 0.5% LI 1.0% LI
0.5 N 5 0.02 ± 0.009 0.02 ± 0.022 0.01 ± 0.000
10 0.03 ± 0.010 0.02 ± 0.004 0.02 ± -0.003
1.0 N 5 0.07 ± 0.005 0.07 ± 0.001 0.06 ± 0.004
10 0.08 ± 0.004 0.08 ± 0.011 0.09 ± 0.002
1.5 N 5 0.06 ± 0.005 0.08 ± 0.007 0.08 ± 0.009
10 0.07 ± 0.021 0.08 ± 0.006 0.09 ± 0.011
1.0H 5 0.02 ± 0.006 0.02 ± 0.002 0.01 ± 0.003
10 0.03 ± 0.009 0.03 ± 0.017 0.02 ± 0.001
2.0H 5 0.02 ± 0.006 0.02 ± 0.002 0.02 ± 0.003
10 0.05 ± 0.003 0.03 ± 0.003 0.02 ± 0.000
3.0H 5 0.03 ± 0.003 0.03 ± 0.011 0.02 ± 0.002
10 0.04 ± 0.003 0.03 ± 0.007 0.04 ± 0.003