Table 2. Average Particle Size, As Determined by Laser Diffraction, Expressed as Sauter Mean Diameter (SMD) and Volume Median Diameter (VMD) of CS, CSMCC, and PMMA Powdersa.

material SMD (μm) VMD (μm)
PMMA 34.6 ± 19.6 290.5 ± 171.6
CS 120.3 ± 21.8b 533.0 ± 32.1b
CSMCC 138.7 ± 53.9b 630.3 ± 39.9bc
a

The values are reported as mean ± SD (n = 3). Dunnett’s multicomparison test was used to compare SMD and VMD of CS and CSMCC with the ones of PMMA:

b

p < 0.05. t-test was used to compare CS and CSMCC:

c

p < 0.05.