Figure 9.

Figure 9

Flow-process of the fabrication of the flexible SLG/AgNWs composite electrode. (a) Deposited graphene on PET. (b) Spin-coating of AgNWs on Graphene-PET; (c) Drying the composite film at 150 °C for 10 min after patterning. (d) Spin-coating of the photoresist, NOA63, (e) Solidification of NOA63 under ultraviolet light for 4 min. (f) Peeling off of the composite film from the PET substrate to obtain the standalone flexible composite electrode.