In vitro degradation results of HADM coated with THA crosslinked using 0.0001%, 0.00075%, and 0.003% H2O2. Alcian blue stained histologic sections showed a continuous THA coating localized on the epidermal surface of HADM at time-zero. THA coatings appeared thinner, particularly in the 0.0001% H2O2 group after 24 and 48h of degradation in 25U/ml hyaluronidase.