Skip to main content
. Author manuscript; available in PMC: 2020 Nov 1.
Published in final edited form as: J Biomed Mater Res B Appl Biomater. 2019 Mar 12;107(8):2664–2672. doi: 10.1002/jbm.b.34357

Figure 7.

Figure 7.

In vivo degradation results showing change in cross-sectional area of THA coatings on HADM. A significant decrease in cross-sectional area was observed between 0–1 week of implantation in the 0.0001% H2O2 (*, p=0.038) and 0.003% H2O2 groups (#, p=0.015).