Figure 2.
(a) The ultimate tensile strength comparison or force taken to rupture the specimen, given in MPa for each specimen group of PDMS A-10 and PDMS 00-30 composites with 0%–4% fibre addition. The error bars represent the standard deviation in each group. (b) Average Young’s modulus comparison for each specimen sample group with 0%–4% fibre addition. The error bars represent the standard deviation in each group.