Skip to main content
. 2019 Nov 6;12(22):3647. doi: 10.3390/ma12223647

Figure 4.

Figure 4

(a) Comparison of force decay of samples measured after 60 s on the 5th loading cycle. The error bars represent the standard deviation in each group. (b) Comparison of the unrecovered deformation observed in all specimens after 60 s at 5 N. The error bars represent the standard deviation in each group.