Skip to main content
. 2019 Nov 7;12(22):3664. doi: 10.3390/ma12223664

Table 4.

Mixture proportions of Labiles Waterglass (LW) grouting materials.

Mix No. Liquid A Liquid B
SS (No.3) (dm3) Water (dm3) Binders (dm3) Water (dm3)
OPC 25 25 10 40
CGM 25 25 10 40

Remarks: Injection pressure: 0.3–0.7 MPa; injection method: 1.5 Shot, double-packer injection.