a) HR‐TEM image of MnGa4 after OER showing porous structure. The Mn 2p XPS spectra (b) and Mn/Ga K‐edge XANES (c–d) spectra of as‐synthesized, as‐deposited, and post OER films of MnGa4 (red arrow indicates oxidation).