The ice adhesion strength for different surfaces in 3 repeated icing tests. For all the surfaces tested, there are no significant changes in the ice adhesion strength during the 3 tests. Lower ice adhesion was achieved on PDMS+PDMS-PEG coatings (PDMS+626 and PDMS+224) than on PEMA-POSS coating. The washed PDMS+626 coating has slightly higher ice adhesion strength than the non-washed counterparts. No apparent change in ice adhesion is observed on the PDMS+224 coating after washing.