Skip to main content
. 2019 Oct 31;9(11):1549. doi: 10.3390/nano9111549

Figure 8.

Figure 8

Logarithmic storage modulus, log (G′), vs. xGnP wt%, adjusted using the percolation model (Equation (2)) at 0.01rad·s−1 and 293.15 K with 0.1% of strain.