Table 1.
Performance comparison of Pd based catalysts on different supporting matrices.
| Sl.No | Name of the catalyst | Onset potential (V vs. SHE) | Tafel slop value (mV/dec) | Medium | Current density; RDE data (mA/cm2) | No. of electrons (n) | Reference |
|---|---|---|---|---|---|---|---|
| 1 | Pd/Activated Carbon | 0.58 | — | 0.5 M HClO4 | 1.1* | — | 33 |
| 2 | Pd/LaFeO3 | 0.66 | 92 | 0.1 M KOH | 3.92 | 2.21 | 34 |
| 3 | Pd/WC-700-m | 0.69 | — | 0.1 M NaOH | 2 | 3.0 | 35 |
| 4 | Pt/C (commercial) | 1.04 | |||||
| PdNi dealloyed | 1.04 | — | 0.1 M HClO4 | — | — | 36 | |
| Pd dealloyed | 0.90 | ||||||
| 5 | NM (Nanotubular Mesoporous) -Pd | 0.90 | 67 | 0.1 M HclO4 | 6.0 | 4 | 37 |
| Pd/C | 0.95 | 88 | 5.0 | ||||
| 6 | Pd/PEDOT | 0.51 | 105 | 0.5 M H2SO4 | 1.8 | 2.8 | This work |
| 7 | Pd/rGO | 0.86 | 121 | — | 2.1 | 3 | |
| Pd/PEDOT/rGO | 0.98 | 152 | 0.1 M KOH | 0.82 | 3.7 |
*Taken from CV data at 0.1 V/s.