. 2019 Aug 9;31(18):7531–7546. doi: 10.1021/acs.chemmater.9b02329

Figure 5.

Figure 5

Plotted data of the (a) σ (chain/nm2) and (b) RF/Dm ratio as a function of the starting molar concentration (M). Both plots report data obtained from experiments conducted with phosphonate-terminated 500 g mol–1 mPEG in DCM at 42 °C with constantly increasing molar concentration of the polymer.