Figure 8.

Figure 8

Membrane obtained after curing a liquid mixture of poly(ethylene glycol) diacrylate (PEGDA) and poly(ethylene glycol) diglycidyl ether (PEGDE) with lithium bis-(trifluoromethanesulfonyl)imide (LiTFSI) and benzoyl peroxide (BPO) at 110 °C for 2 h. The mass ratio of PEGDE:PEGDA was 1:1 and the molecular weight of PEGDE 500 g mol−1. The chain length of PEGDA was determined by its molecular weight of 1000 g mol−1. (a) This membrane could be bent without cracking. (b) The cycling performance of LiFePO4//Li battery with this membrane as the electrolyte. The test was conducted at 0.2C and 55 °C. Reproduced with permission from [274]. Copyright 2018 Elsevier.