Skip to main content
. 2019 Nov 24;12(23):3884. doi: 10.3390/ma12233884

Figure 6.

Figure 6

The electroplated samples’ isothermal treatment at different times at 700 °C: (a) surface microhardness and mass loss; (b) friction coefficients curves. (c,d) show the worn surface SEM and laser confocal morphologies of heat treatment for 3 and 7 h, respectively.