Figure 5.

Figure 5

The X-ray diffraction (XRD) results of the sintered Si3N4/n-SiC ceramics at different sintering temperatures (holding time for 10 min), (a) 1400 °C, (b) 1500 °C, (c) 1600 °C, and (d) 1700 °C.