. 2019 Dec 2;12(23):3994. doi: 10.3390/ma12233994

Figure 9.

Figure 9

XRD pattern of the MSC-Scaffold pre-prototype coated with a layer of CaP deposited by ECDV=const at VECD = −5.00 V (followed by 48 h immersion in SBF).