Table 1. List of Samples Studied in This Paper with Their Nickname, Fabrication Method (First or Second Generation), Total Sample Cross Section Including Substrate As (μm)2, Figure of Merit (with Crystal Cross Section Acr = (12μm)2), and Pixel Volume in the Tomography Scans Vpix (nm3)a.
name | fabrication method | As | F | Vpix |
---|---|---|---|---|
good | 1 | 1460(60) × 730(20) | 86(4) | 203 |
bad | 1 | 480(20) × 410(30) | 37(3) | 203 |
ugly | 2 | 500(50) × 530(20) | 43(5) | 103 |
Numbers between parentheses are estimated error margins.