Skip to main content
. 2019 Dec 16;52(24):9427–9444. doi: 10.1021/acs.macromol.9b02085

Figure 14.

Figure 14

Comparison of linear viscoelasticity of supramolecular polymers with different contents of UPy (3, 5, and 10%) as side groups (sticker) and precursor molecular weights (a) lower (42.5 kg mol–1), (b) close to (76.4 kg mol–1), and (c) above critical molecular weight Mc (165.4 kg mol–1). Reproduced with permission from ref (49).