Representative case studies on Mg-based bone screws used for fixation of autologous bone grafts or bone fracture in China.

Mg and Mg alloy Animal model Size Implantation period Ref Published time
AZ31B/silicon-containing coating rabbit femur shaft D 2.6 mm*L 6.5 mm 1, 4, 12, 21 W [29] 2014
High purity Mg rabbit
femoral intracondylar fracture model
D 2.7 mm *L 27 mm 4, 8, 16, 24 W [30] 2015
Mg-Nd-Zn-Zr/brushite coating (JDBM-DCPD) rabbit mandible D 2 mm*L 4.6 mm 18 M [10] 2016
Mg-Nd-Zn-Zr/uncoated (JDBM) goat femoral condyle fracture model D 4.5 mm*L 45 mm 18 M [11] 2018
JDBM-DCPD
Mg–6Zn-0.5Sr rabbits tendon graft fixation D 3 mm*L 8 mm 6, 12, 16 W [31] 2018