Figure 6.

Figure 6

The Thermoelectric Properties of Silver Selenide Films before and after Being Annealed

The electrical resistivity (A), Seebeck coefficient (B), and power factor (C) at 303 K of silver selenide films before and after being annealed, and the errors of these three parameters are ±5%, ±7%, and ±14%, respectively. This figure is related to Figure S5.