Skip to main content
. 2019 Nov 30;23(1):100753. doi: 10.1016/j.isci.2019.100753

Table 2.

The Power Factors at Around 300 K of Annealed Ag2.3Se Film in This Work and Representative Thermoelectric Bulk Materials and Flexible Films

Sample Power Factor (μWm−1K−2)
Flexible annealed Ag2.3Se film 2451 ± 364 (this work)
5%Te/Ag2Se bulk materials 1800 (Lim et al., 2019)
Ag2Se1.06 bulk materials 3010 (Mi et al., 2014)
Ag2Se film on glass substrate 2440 ± 192 (Perez-Taborda et al., 2018)
Flexible nylon-supported Ag2Se film 987 ± 104 (Ding et al., 2019)
Flexible nylon-supported Cu1Ag4Se3 film 2232 (Lu et al., 2019)
Bi2Te2.7Se0.3 film on glass fiber 2077 (Shin et al., 2017)