. 2017 Mar 10;6(2):147–159. doi: 10.1007/s40192-017-0093-4

Fig. 4.

Fig. 4

An example of the typical evolution in 2D SAXS patterns with increasing strain for a tensile specimen of LLDPE2.2a. Strain is applied in the vertical direction with a tensile deformation rate of 25.4 mm/min. The numbers indicate the SAXS pattern number; an interval of 3 s between consecutive patterns is strictly maintained. Every tenth image is displayed for clarity. The intensity is log scaled to highlight the characteristic features in the SAXS evolution with strain (Color figure online)