. 2019 Dec 6;12(24):4075. doi: 10.3390/ma12244075

Figure 2.

Figure 2

Figure 2

Microstructure and porosity of the NiTi46 alloy SPS consolidated at various temperatures: (a) 900 °C-perpendicular, (b) 900 °C-longitudinal, (c) 1000 °C-perpendicular, (d) 1000 °C-longitudinal, (e) 1100 °C-perpendicular, and (f) 1100 °C-longitudinal direction.