Differential scanning calorimetry (DSC) analysis.

Material Tg Tm Td Hg Hm Hd
ABS 100.2 111.8 131 430.4 -- 3.0 (combined peak) 445.8
PP 170.6 458 82.5 148
PE-g-MAH 108.6 475.8 27.22 164.5
ABS/PP 94.1 132.7 (ABS) 163.4 (PP) 427.5 2.251 1.09 (ABS) 4.6 (PP) 489.5
ABS/PP/PE-g-MAH pellets 93.5 128.7 (ABS) 163.6 (PP) 424.8 2.464 3.61 (ABS) 2.72 (PP) 488.8
ABS/PP/MAH combination 1 91.6 127.7 (ABS) 163.7 (PP) 425.9 2.53 1.69 (ABS) 4.075 (PP) 525.6
ABS/PP/MAH combination 10 93.8 127.4 (ABS) 163.5 (PP) 426.1 2.502 2.93 (ABS) 4.39 (PP) 529.4
ABS/PP/MAH combination 27 -- 109.3 (ABS) 129.3 (ABS) 163.9 (PP) 427.1 1.37 (ABS) 2.86 (ABS) 4.03 (PP) 500