. 2019 Dec 10;12(24):4141. doi: 10.3390/ma12244141

Figure 4.

Figure 4

Typical speckle fringes of (a) before heating (at 22.0 °C), and (b) after heating at the temperature of 24.5 °C under no initial stress condition.