Skip to main content
. 2020 Jan 6;12:1–8. doi: 10.2147/CCIDE.S219705

Table 2.

Failure Type And Percentage Of Fracture Of Zirconia And Resin Composite Discs

Groups Control TCL Water Esterase
No Storage 2 Weeks 24 Weeks 48 Weeks 2 Weeks 24 Weeks 48 Weeks
CON IF 100% IF 100% IF 100% IF 100% IF 100% IF 100% IF 100% IF 100%
GB IF 60%
RC 40%
IF 70%
RC 30%
IF 80%
RC 20%
IF 90%
RC 10%
IF 100% IF 90%
RC 10%
IF 100% IF 100%
LAS IF 70%
RC 30%
IF 80%
RC 20%
IF 80%
RC 20%
IF 100% IF 100% IF 80%
RC 20%
IF 100% IF 100%
SIE IF 20%
RC 30%
CO 50%
IF 30%
RC 30%
CO 40%
IF 40%
RC 40%
CO 20%
IF 60%
RC 40%
IF 70%
RC 30%
IF 50%
RC 40%
CO 10%
IF 80%
RC 20%
IF 90%
RC 10%

Abbreviations: IF, interfacial; RC, cohesive in resin cement; CO, cohesive in resin composite.