Figure 1.

Figure 1

Scanning electron microscope (SEM) images of poly-ε-caprolactone (PCL)-ref, PCL–COOH, and PCL–TiCaPCON nanofibers before (left column) and after biomimetic mineralization for 1, 3, 7 and 14 days.