Skip to main content
. 2019 Dec 6;9(12):1737. doi: 10.3390/nano9121737

Table 4.

Mechanical self-healing efficiency of various hydrogels after different healing times.

Sample f1
After 2 h Healing
f1
After 4 h Healing
f1
After 6 h Healing
TOCNF/PAA 28.9% 64.6% 73.5%
TOCNF/PAA-PPy-0.2 71.3% 84.1% 95.3%
TOCNF/PAA-PPy-0.4 81.4% 91.5% 97.5%
TOCNF/PAA-PPy-0.6 73.0% 87.9% 98.3%
TOCNF/PAA-PPy-0.8 58.4% 87.0% 96.7%