. 2019 Nov 20;9(12):1645. doi: 10.3390/nano9121645

Figure 3.

Figure 3

Cross-sectional SEM images of ZnO layer formed on the FTO glass for (a) 4 h, (b) 6 h, (c) 8 h, and (d) 10 h growth time.