Table 1.

Formation enthalpies for TiMgN2 crystallized in five different structures

TiMgN2
ICSD id Formation enthalpy (eV/atom) Nitride example
82537 − 1.299 SrZrN2 (NaCrS2)
98663 − 1.260 LiUN2
74904 − 1.005 BaZrN2 (BaNiS2)
15144 − 1.234 ZnGeN2 (NaFeO2-beta)
74791 − 1.222 BaCeN2, inverse-MAX

The ICSD id is the entry identification number which the structure is based on. The nitride examples represent actual existing ternary compounds and the respective structures which they crystallize in