Skip to main content
. Author manuscript; available in PMC: 2021 Jan 1.
Published in final edited form as: Acta Biomater. 2019 Nov 8;101:227–236. doi: 10.1016/j.actbio.2019.11.009

Figure 2.

Figure 2.

The effect of degradability on hMSC spreading and proliferation in RGDS-functionalized MAP hydrogels. a) Maximum intensity Z- projection of cytoskeleton staining of hMSCs cultured in MAP hydrogels after 2 and 8 days. Green represents F- actin and blue represents nuclei. Scale bars are 100 μm. b) Quantification of cell number. c) Quantification of cell volume. * comparison factor: degradability; # comparison factor: time. * indicates p < 0.05, *** and ### indicate p < 0.0001, Two-way ANOVA and Tukey’s multiple comparisons test.