Skip to main content
. 2019 Dec 4;11(12):2010. doi: 10.3390/polym11122010

Table 2.

Particles size, polydispersity index (PDI) and zeta potential of α- or β-chitosan nanoparticles prepared from chitosan with different set of deacetylation degree (%DD) and molecular weight (MW) combinations respectively.

Samples Particles Size (nm) PDI * Zeta Potential (mV)
aNP1 169.23 ± 3.33d 0.314 ± 0.015a 23.07 ± 1.15c
aNP2 165.03 ± 2.57d 0.271 ± 0.014a 24.43 ± 0.81bc
aNP3 332.20 ± 15.85a 0.168 ± 0.101bc 26.33 ± 2.91b
bNP1 192.50 ± 1.91c 0.248 ± 0.012ab 24.83 ± 0.49bc
bNP2 170.13 ± 2.29d 0.152 ± 0.011c 25.40 ± 0.56bc
bNP3 232.30 ± 3.27b 0.098 ± 0.052c 30.57 ± 0.64a

* PDI = polydispersity index. All the data represent the mean with standard deviation (n = 3). a,b,c,… The different letters present statistical difference (p < 0.05). Where: a = α-chitosan, b = β-chitosan, NP = chitosan nanoparticles, 1 = low %DD and high MW, 2 = medium %DD and medium MW, and 3 = high %DD and low MW.