Skip to main content
. 2019 Dec 9;19(24):5409. doi: 10.3390/s19245409

Figure 3.

Figure 3

CV of 2.5 mM ferricyanide in PBS buffer on various electrodes assayed at a scan rate of 0.1 V s−1. Electrochemical surface area for GSPE is (0.149 ± 0.009) cm2 (roughness factor of 1.19) and for activated GSPE is (0.171 ± 0.010) cm2 (roughness factor of 1.36).