Skip to main content
. 2019 Dec 11;11(12):2052. doi: 10.3390/polym11122052

Figure 3.

Figure 3

SEM images of nanofibers under different conditions of the spinning process. (A) 55 kV, 10 wt %; (B) 60 kV, 10 wt %; (C) 65 kV, 10 wt %; (D) 55 kV, 11 wt %; (E) 60 kV, 11 wt %; (F) 65 kV, 11 wt %; (G) 55 kV, 12 wt %; (H) 60 kV, 12 wt %; (I) 65 kV, 12 wt %. Scale bar = 5 μm.