Skip to main content
. 2019 Dec 11;11(12):2062. doi: 10.3390/polym11122062

Figure 10.

Figure 10

MM images of a fiber scaffold sample fabricated at a relative collector velocity of 0.4 m/s. The result is comparable to the MM of a diffuse scattering sample, indicated on the right side of Figure 5. The data shows that the sample is homogeneous.