. 2019 Nov 29;11(12):1967. doi: 10.3390/polym11121967

Figure 5.

Figure 5

Time evolution of pyrolysis product distributions of styrene-butadiene rubber at different temperatures, (a) 1500 K, (b) 2000 K, (c) 2500 K and (d) 3000 K.