Characteristics of Ti-PET and Sb-PET resins at isothermal temperatures of 195 °C and 205 °C. (a) The total isothermal crystallization peak; (b) The variation in fractional crystallinity (Xt); (c) The linear plot of log[−ln(1 − Xt)] versus log(t).