Table 2.

Characterization results for Titanium based (Ti-) and antimony-based (Sb-) PET resins, and respective as-spun fibers obtained at a spinning velocity of 4 km/min.

Sample IV (dl/g) GPC ICP TGA 1
M n M w Mw/Mn Sb (ppm) 99% 90%
Ti-PET Resin 0.634 (0.602 2) 4153 11,235 2.70 - 369 398
Sb-PET Resin 0.630 (0.592 2) 4124 10,986 2.66 244 (163 2) 372 402

1 The temperature at weight loss of 99 wt % and 90 wt %. 2 Data of as-spun fiber.