Skip to main content
. 2019 Nov 22;20(1):1118–1130. doi: 10.1080/14686996.2019.1694841

Figure 7.

Figure 7.

(a) Schematic PSC fabrication process on the double HTL of ta-C and NiO and cross-sectional TEM image obtained from PSC with the NiO/ta-C/ITO anode. (b) Enlarged TEM images obtained from A (Ag/BCP/PCBM/CH3NH3PbI3 interface), B (CH3NH3PbI3/NiO/ta-C/ITO interface), C (NiO/ta-C/ITO), and D (ta-C), respectively.