adsorbent surface area (m2/g) adsorption time (min) Adsorption capacity (mg/g) initial sulfur content (ppm) refs
microwave-synthesized carbon nanotubes 171.0 60 21.50 250 (61)
ACTD 493.0 90 8.60 150 (15)
ACWS 1570.0 30 47.10 220 (62)
ACFH-Cu+2 1090.0 480 19.00 330 (63)
mesoporous carbon-silica nanocomposite via copper modification 276.0 2880 13.95 960 (64)
carbon aerogels 741.0 96 15.10 250 (65)
AC/γ-Fe2O3 nanocomposite 363.0 40 38.00   (66)
magnetic mesoporous carbon 705.0 60 62.00 1000 (67)
PMAC 1/3 2038.0 60 84.67 500 this work
PMAC 1/4 2784.0 60 74.97 500 this work