E-SEM micrographs of fractured surfaces of carbon flax hybrid composites: (a) image showing carbon fibre aligned on the top and bottom surfaces and flax being observed in the middle; (b) carbon fibre observed properly aligned, some defects on the surface of carbon fibre are visible and some delamination is also visible; and (c) flax fibres observed clustered in the middle.