Skip to main content
. 2020 Jan 1;13(1):176. doi: 10.3390/ma13010176

Figure 3.

Figure 3

Open circuit potential plots of non-modified (Ti6Al4V), anodized in 1 M H3PO4 (Ti6Al4V compact) and anodized in ethylene glycol (99%) + 0.6 wt. % NH4F (Ti6Al4V nanotubular) before and after implantation into pig’s Th8 vertebra by the Magerl technique measured in 0.9% NaCl (A) and 0.01 M PBS (B) during 1200 s.