Skip to main content
. 2020 Jan 31;11:643. doi: 10.1038/s41467-020-14505-8

Fig. 2. SEM analysis of the lithium anode.

Fig. 2

Top view SEM images of lithium stripping after three cycles at 0.5 mA cm−2 for 0.4 h with untreated electrolyte (a, b), with PEGDME (c, d), and OP-10 additives (e, f) (Scale bars: a, c, e 100 μm; b, d, f 20 μm).