Fig. 1.

Fig. 1.

(a) Picture and (b) Schematic of experimental setup for room temperature fast fracture tensile testing of coated and uncoated single tow ceramic matrix minicomposite samples where the minicomposite is mounted in steel pins in the gripping fixtures of an Instron testing machine along with 2 acoustic emission sensors and 4 electrical resistance probes.