Published in final edited form as: J Eur Ceram Soc. 2017 Aug;37(10):3241–3253. doi: 10.1016/j.jeurceramsoc.2017.03.065

Fig. 3.

Fig. 3.

SEM image of slurry coated minicomposite with various cycles (a. with 10 coating cycles; b. with 3 coating cycles) 10 cycles coating performed larger dry cracks and thicker coating layer compared with 3 cycles.