Table 3.

Comparison of amount of natural enamel wear against polished yttrium–tetragonal zirconia polycrystals crowns (Group 1) with enamel wear against natural antagonist (Control group)

Groups Mean (μm) SD SE Student t-test P, significance
Enamel wear against Polished Y-TZP crowns (group 1) 42.0 6.66 1.72 3.205 0.017, significant statistical difference
Enamel wear against natural antagonist (control group) 34.68 6.49 1.68

P>0.05: Not significant, P<0.05: Significant, P<0.001: Highly significant. Y-TZP: Yttrium–tetragonal zirconia polycrystals, SD: Standard deviation, SE: Standard error