Skip to main content
. 2020 Jan 9;13(2):312. doi: 10.3390/ma13020312

Figure 5.

Figure 5

The hot processing maps of homogenized TAZ321 alloy at the true strain of (a) 0.2, (b) 0.4, (c) 0.6, and (d) 0.8.